Case Studies

WJE Report 1

Resilience - The resilience defined by Tex-618-J is the ratio of the maximum displacement plus the height of the cube after testing minus the height of the cube before testing to the maximum displacement, where in this case the maximum displacement was 0.1 in... read more...

WJE Report 2

The patching compound was produced by combining equal volumes of Component A, which was a dark brown liquid with viscosity approximately equal to water, Component B, which was gray and had a higher viscosity than A, a Flow Mix catalyst and sand. Mixing was done in the one-gallon buckets in which all materials were supplied in pre-packaged containers... read more...

WJE Report 3

The patching compound was produced by combining equal volumes of Component A, which was a dark brown liquid having a viscosity approximately equal to water, Component B, which was gray and had a higher viscosity than A, a Flow Mix catalyst, and sand... read more...